Before treatment the figure appears in good condition, but a closer look reveals minor areas of corrosion in the following images
Before treatment: the surface shows signs of minor, unsightly corrosion
Before treatment: the surface shows signs of minor, unsightly corrosion
The surface is rinsed of the acid treatment with water at normal hose pressure to ensure all residues are removed
After treatment: the corrosion is reduced and rust staining is not evident
After treatment: the corrosion is reduced and rust staining is not evident
After treatment the overall sculpture appears more uniform without rust stains